Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3WG13 BK00102 - PA6-GF63 - BASF

Material Data Center offers the following functions for Ultramid® B3WG13 BK00102:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Ultramid® B3WG13 BK00102 is a 63% glass filled, injection molding, high modulus Polyamid designed to have high strength and stiffness for metal replacement applications. It also has excellent moldability and outstanding surface appearance.

Applications:
Potential applications are mirror brackets, fuel lids, gas-assisted steering wheel inserts, ski bindings and bike rack clamps.
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 22400 / - MPa ISO 527
Tensão na ruptura 235 / - MPa ISO 527
Deformação na ruptura 2 / - % ISO 527
Resistência ao impacto Charpy , +23°C 90 / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 90 / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 15 / - kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 13 / - kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 220 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 214 / * °C ISO 75-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.5 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Flamabilidade a espessura h HB / * class IEC 60695-11-10
Espessuras do tubo de teste 3.0 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1740 / - kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 80 °C -
Umidade do processamento ≤0.03 % -
Temperatura da massa 300 - 320 °C -
Temperatura do molde 80 - 95 °C -
Diagrama
Viscosidade - taxa de cisalhamento , Ultramid® B3WG13 BK00102, PA6-GF63, BASF
Tensão de cisalhamento - taxa de cisalhamento , Ultramid® B3WG13 BK00102, PA6-GF63, BASF
Tensão - deformação , Ultramid® B3WG13 BK00102 (dry), PA6-GF63, BASF
Tensão - deformação , Ultramid® B3WG13 BK00102 (cond.), PA6-GF63, BASF
Módulo secante - deformação , Ultramid® B3WG13 BK00102 (dry), PA6-GF63, BASF
Módulo secante - deformação , Ultramid® B3WG13 BK00102 (cond.), PA6-GF63, BASF
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos, Negro
Características especiais
Estável contra o calor
Disponibilidade regional
América do Norte
Outras informações
Moldagem por injeção
PREPROCESSING
Max. Water content: 0.03%
Although Product is supplied in sealed containers, drying is recommended in applications requiring optimum surface aesthetics. A dehumidifying or desiccant dryer operating at 80 °C (176 °F) is recommended. Drying time is dependent on moisture level.
Further information concerning safe handling procedures can be obtained from the Material Safety Data Sheet. Alternatively, please contact your BASF representative.

PROCESSING
Melt Temperature 300-320 °C (572-608 °F)
Mold Temperature 80-95 °C (176-203 °F)
Injection and Packing Pressure 35-125 bar (500-1500psi)
Rear Zone 275-300 °C (527-572 °F)
Center Zone 285-310 °C (545-590 °F)
Front Zone 300-325 °C (572-617 °F)
Nozzle 300-325 °C (572-617 °F)

This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics arecritical, a mold surface temperature of 80-95 °C (176-203 °F) is required.

Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.

Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage.

Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com